4dhcpmingchen

【Origin Pic】

【Applicable scope】

Suitable for various types of pure cotton, polyester/cotton fabrics, both knitted and woven.

【Product characteristics】

Appearance: Light yellow flakes

Ionicity: weak cation

PH value: 4-5.5 (10% diluent)

Ingredients: Fatty acids, organic amine compounds

【Characteristics and performance】

The outstanding soft and fluffy texture is suitable as a post finishing softener for various needle and woven fabric dyeing factories.

Excellent salt, alkali, and hard water resistance performance

The product has low viscosity, low foam and low yellowing.

Dyeing factory specific film TS-C760

Product Description

The special film TS-C760 for dyeing factory has outstanding properties such as low viscosity, low foam, high compatibility, etc. It is suitable for various knitting and woven fabrics dyeing factory to be used as post finishing softener. The handle is mainly soft and has excellent bulkiness

Usage

Impregnation method

Dosage: 2% -5% (o.w.f) (10% diluent)

Process: Room temperature~40 ℃ x (5-30) min

Bath ratio: 1:6~1:20

Immersion and rolling method (one immersion and one rolling or two immersion and two rolling)

Dosage: 20-50g/L (10% diluent)

Rolling residual rate (with liquid content): 60% -100%

Chemical method

High temperature hardening material: Put the soft film into room temperature water in a ratio of 5% -10%, stir while raising the temperature by 65 ℃ -75 ℃, and then keep it warm and stir for 20-30 minutes until the slurry is uniform. Seal it (to prevent the dilution solution from scaling) and cool it for later use.

matters needing attention

If the packaging is opened, please use it up as soon as possible. If it is not used up, it needs to be sealed for next use. It is recommended not to mix it with other products.

Packaging and storage

Non dangerous goods, 25KG/pack, sealed and stored in a ventilated and cool place, avoiding high temperature and exposure to sunlight, with a storage period of six months.

Recommended product combinations

Various types of pure cotton, polyester/cotton fabrics: silicone oil TS-8848/8868 film TS-C760

Dosage: silicone oil TS-8848/8868: impregnation method: 2-4% (o.w.f) (20% lotion) dip rolling method: 20-50g/L (20% lotion)

Dosage: Soft film TS-C760: Immersion method: 3-5% (o.w.f) (10% diluent) Immersion rolling method: 20-50g/L (10% diluent)